Product overviews
Three-Point Bend Flexural Strength (after crystallization) 420±60 MPa
Density (after crystallization) 2.46-2.52 g/cm
3
Thermal Expansion Coefficient (after crystallization): 10.5*10
-6
/K (50-500°C)
Linear Shrinkage Rate: 0.10-0.26%
Vickers Hardness (after crystallization): 6500±200 MPa
Elastic Modulus (after crystallization): 50±10 GPa
Fracture Toughness (after crystallization): 2.8-3.8 MPa m
-1/2
Chemical Solubility (after crystallization): < 100 μg/cm
2