Item
|
666,7560,C grade
|
Place of Origin
|
China
|
Main Raw Material
|
Acrylic
|
Usage
|
Construction
|
Product Name
|
Heavy Duty Glue
|
Package
|
300mL/360g/pc,24pcs/carton
|
Feature
|
High viscosity
|
Function
|
multifunction
|
Type
|
manual
|
Keywords
|
manual
|
Brand
|
OEM Customized
|
Shelf Life
|
18months
|
Phenomenon
|
Possible Reasons
|
Solutions
|
Weak adhesion
|
1. Not using the right type of hot-melt glue
2.Wooden board is too dusty
3.Edge banding is polluted
4. Primer coating is not even or
no primer on the edge banding
5. Not enough pressure on the edge bander
|
1.Change a suitable glue item
2.Clean the wood board
3.Change edge banding
4.Change edge banding withgood primer coating
5.Adjust pressure
|
Drawing polluting plank
|
1.Not using the right type of hot-melt glue
2.The temperature is too high.
3.Too much glue coating.
4.Defects in coating cylinder so
the gluecannot be applied evenly |
1.Change a suitable glue item
2.Lower down the temperature
3.Adjust coating quantity
4.Change another cylinder
|
Adhesive with thick lines
|
1.Not using the right type of adhesive
2.The wooden board is not cut smoothly
3.The edge banding is not in good shape
4.Uneven pressure on the pressureroller of edge bander
5.Not enough pressure on edge bander
6.Too much glue coating amount,so glue spill out
|
1.Choose another glue item
2.Do better neat cutting on the wooden board
3.Change better quality edgebanding
4.Change pressure roller
5.Adiust pressure on the roller
6.Adiust glue amount
|