International code name
|
SK35
|
SK36
|
SK37
|
SK38
|
SK40
|
Al2O3/%
|
≥48
|
≥55
|
≥65
|
≥75
|
≥80
|
Fe2O3/%
|
≤2
|
≤2
|
≤2
|
≤2
|
≤2
|
Refractoriness
|
≥1750 °C
|
≥1770 °C
|
≥1790 °C
|
≥1790 °C
|
≥1790 °C
|
Apparent porosity
|
≤22%
|
≤22%
|
≤23%
|
≤23%
|
≤21%
|
Cold crushing strength
|
≥39Mpa
|
≥44Mpa
|
≥49Mpa
|
≥54Mpa
|
≥65Mpa
|
Refractoriness under load (0.2MPa)
|
≥1420 °C
|
≥1470°C
|
≥1500 °C
|
≥1520 °C
|
≥1530 °C
|
Reheating Linear Change (1500°C 2h) %
|
+0.1~ -0.4
*1450°C |
+0.1~ -0.4
|
+0.1~ -0.4
|
+0.1~
-0.4 |
+0.1~ -0.4
|