Property
|
Test Method
|
Reference rang
|
Unit
|
|
Molecular Weight
|
|
1.5-9 million
|
|
|
Density
|
ISO 1183-1:2012/DIN53479
|
0.92-0.98
|
g/cm³
|
|
Compression Strength
|
ISO 604:2002
|
≥32
|
Mpa
|
|
Tensile Strength
|
ISO 527-2:2012
|
≥22
|
Mpa
|
|
Elongation at break
|
ISO 527-2:2012
|
≥300
|
%
|
|
Dynamic Friction Coefficient
|
ASTM D 1894 /GB 10006-88
|
≤0.18
|
|
|
Notched impact strength (charpy)
|
ISO 179-1:2010/GB/T 1043.1-2008
|
≥100
|
kJ/m2
|
|
Abrasion wear index
|
ES-X60210-2008
|
≤30
|
mg
|
|
Vicat softing point
|
ISO 306:2004
|
≥80
|
ºC
|
|
Hardness Shore-D
|
ISO 868:2003
|
61-66
|
D
|
|