Typical general characteristics
|
Inspection
Method
|
Value
|
|
|
|
|
||||
Product data(Catalyzed A+B)
|
Method
|
X805
|
X810
|
X815
|
X710
|
X720
|
||||
(catalyzed A+B)
|
|
|
|
|
|
|
||||
Hardness
|
Shore A
|
5
|
10
|
15
|
10
|
20
|
||||
Mix ratio
|
A:B
|
1:1
|
1:1
|
1:1
|
1:1
|
1:1
|
||||
Color
|
/
|
Translucent
|
Translucent
|
Translucent
|
Translucent
|
Translucent
|
||||
Pot life
|
25℃(77F)
|
5-30 mins
|
5-30 mins
|
5-30 mins
|
5-30 mins
|
5-30 mins
|
||||
Curing time
|
25℃(77F)
|
1-4 hours
|
1-4 hours
|
1-4 hours
|
1-4 hours
|
1-4 hours
|
||||
Viscosity
|
mPa.s
|
2000±1000
|
2500±1000
|
3000±1000
|
4000±1000
|
6000±2000
|
||||
Tear strength
|
KN/m
|
≥12
|
≥15
|
≥18
|
≥7
|
≥5
|
||||
Tensile strength
|
MPa
|
≥2.5
|
≥3.5
|
≥4.5
|
≥2.5
|
≥4.0
|
||||
Elongation
|
%
|
≥450
|
≥450
|
≥450
|
≥650
|
≥560
|
||||
Shrinkage
|
%
|
≤0.1
|
≤0.1
|
≤0.1
|
≤0.1
|
≤0.1
|