Test project
Unit
PP
PE
E nvironmental stress cracking
h
/
≥800
Low temperature brittleness
° C
≤ -23
≤ -50
Microcal softening temperature
≥ 142
≥ 112
Oxidation induction time
min
≥ 20
≥ -23
T ensile yield strength
Mpa
≥ 23.0
≥ 20.0
Tensile strength at weld
N/cm
≥ 100
Tensile strength at the edge
≥ 200
Tensile strength in the middle
≥ 120